Recertification of in-process control and quality management system of welding procedures of plant for steelwork production UTEM-ZMK

30.05.2019

International certification body TÜV Thüringen e.V. conducted audit of welding production of UTEM-ZMK LLC as per standards ISO 3834 and EN 1090, that allows it marks its products with CE mark.

Upon results of recertification the plant performed upgrade to higher execution level EXC3 and once again confirmed that its in-process control and quality management system of welding procedures complies with requirements of European standards.